From Figure 2 , it becomes apparent that the minimum torque M L of both SBR- as well as NBR-based compounds show an increasing trend with increasing content of the biopolymer.
← all excerpts
Sulfur and Peroxide Cross-Linking of Lignosulfonate-Filled Compounds Based on Acrylonitrile-Butadiene Rubber and Styrene-Butadiene Rubber.
2
—
—
The sentences
With the exception of the compounds based on SBR cured with the sulfur system, the optimum cure time t c 90 showed a decreasing trend with increasing content of lignosulfonate ( Figure 7 ).