a decreasing trendno p-value reported
In terms of quantifying residual austenite, analyses were conducted on the austenitized specimens using XRD, as shown in Figure 13 , retained austenite (RA) volume fraction revealed a decreasing trend after cryogenic treatment, reducing from 9.53% in the CHT sample to 8.43% after 2 h of immersion (CT2/T2) and further to 6.51% after 20 h of immersion (CT20/T2).