However, both the flexural strength and flexural modulus of HA/PLLA composites showed a decreasing trend when the processing temperature was above 140 °C or the pressure exceeded 250 MPa.
← all excerpts
Bioresorbable High-Strength HA/PLLA Composites for Internal Fracture Fixation.