It can be seen that with the increase of the number of freeze–thaw cycles, the pores of each layer inside the red-bed sandstone show an increasing trend.
← all excerpts
Macro and micro damage characteristics of Red-bed sandstone in Urumqi under freeze-thaw cycles.
2
—
—
The sentences
With the increase of the number of freeze–thaw cycles, the pore volume and porosity of the red-bed sandstone samples show an increasing trend, and the material volume and total volume show a decreasing trend.