As shown in Figure 13 , as the temperature gradually increases from low to room temperature and then to high temperature, the peel strength against steel of three test strips of Formula 4# internal protection material all show a decreasing trend.
← all excerpts
Research on High-Performance Underwater-Curing Polymer Composites for Offshore Oil Riser Pipes.