After undergoing 5,000 and 10,000 thermocycles, the SBS values of AI (28.85 ± 7.57/26.28 ± 3.85/17.73 ± 2.57 MPa) and RU (30.95 ± 4.53/36.18 ± 3.64/16.01 ± 3.20 MPa) exhibited a decreasing trend.