K 2 O shows a decreasing trend in all samples after activation, more pronounced in the Kabala samples (from 0.16 to 0.13%).
← all excerpts
Impact of High Energy Milling and Mineral Additives on a Carbonate-Quartz-Apatite System for Ecological Applications.
1
—
—