The ash content of SR-CNF prepared through OA–water pretreatment shows a decreasing trend, with the char residue at 500 °C decreasing from 21.0% to 8.5% as the concentration of OA increases ( Table 1 ).
← all excerpts
Seaweed residue as a low-cost source for producing cellulose nanofibrils with ultraviolet shielding properties.
1
—
—