Both the surface CRS and its affected depth exhibit a decreasing trend with increasing pulse width.
← all excerpts
Experimental and Simulation Study on Residual Stress of Pure Copper Welded Joint by Laser Shock Peening.
2
—
—
The sentences
Figure 12 a exhibits an increasing trend in the CRS on the weld surface as the overlapping rate is increased.