Fig 8 shows that when the skeleton structure of the SMA mixtures was still forming ( VCA mix > VCA DRC(n=25) ), the shear strength and dynamic stability of the SMA mixtures exhibited an increasing trend as the VCA mix of the SMA mixtures decreased.
← all excerpts
Optimization of skeleton structure discrimination standard for SMA-13 mixture based on high-temperature performance.