, , The normalized pre-edge intensity of MnFeCoNiCuO x showed a decreasing trend as Fe (0.195) > Mn (0.105) > Co (0.093) > Ni (0.025) > Cu (0); the pre-edge intensity of MnCoNiCuZnO x : Mn (0.124) > Co (0.113) > Ni (0.023) > Cu (0).