For the Permalloy core material, the loss factor at 100 kHz was 0.018 and at 1 MHz was 0.185, so there was an increasing trend for higher frequencies.
← all excerpts
Partial Discharge Activity Inductive Sensors and the Application of Magnetic Materials.