The E corr of the alloy shows a decreasing trend, with i corr in CE conditions (Table S1) being 10 2 times higher than in quiescent conditions. 3.2.4 EN tests Fig. 13 depicts the electrochemical EPN and ECN signals in synthetic seawater for fresh samples and after CE of the overlapping area and the substrate.