All samples exhibit an increasing trend in \documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$\Delta R/R_0$$\end{document} , which is related to increased LM oxidation caused by the straining.
← all excerpts
Process and property assessment of liquid metal spray deposition towards scalable and reliable stretchable electronics.