There was an increasing trend in the flexural load from SMSR to DSM composites, which ranged from 90 to 171 N, and the increased flexural strength varied from 58 to 110 MPa.
← all excerpts
Development of hybrid fiber-reinforced vinyl ester composites for civil and automotive applications.