From Figure 7(a) , it can be seen that under the heating condition of 200 °C, the pyrolysis rate in the test chamber shows an increasing trend from 0 to 35 minutes, gradually rising from an initial rate of 0 mg/min to around 4.5 mg/min, with the maximum heat release occurring at 30 minutes.