Residual mechanical and self-sensing properties of polypropylene fiber-reinforced waste glass aggregate UHPS after high-temperature exposure.

Sci Rep · 2025 · PMC12635240 · PMID 41266520

1
hedged sentence
closest p
boldest claim

The sentences

an increasing trendno p-value reported
Sensitivity to bending exhibited an increasing trend during the initial cracking stage, but high temperatures exacerbate nonlinear fluctuations and noise interference, leading to unstable sensing responses. “Sensing capability begins to degrade notably after 400 °C, with weakened resistivity–stress correlation, and is significantly weakened at 800 °C”.

also in 63,971 other papers

Quoted from the open-access full text in Europe PMC under the licence the publisher applied. The sentence is reproduced exactly as published; the emphasis is ours.