However, when the temperature increased to 1100 °C, the grain size showed a decreasing trend.
← all excerpts
On the Hardening and Softening Behaviors of Additively Manufactured and Forged Inconel 718 Alloys Under Non-Isothermal Heat Treatments.
2
—
—
The sentences
When heated at a rate of 5 °C/min, the volume fractions of the precipitated phases are 1.1%, 1.3%, and 1.5%, respectively, showing an increasing trend with temperature ( Figure 9 a–c).