As summarized in Table 2 , SR/m-POSS showed higher tensile strength and elongation at break than SR/POSS composite, with p < 0.001 for both properties, indicating a highly significant advantage for SR/m-POSS composite.
← all excerpts
Modification of Octavinyl POSS and Its Effect on the Mechanical Properties and Thermal Stability of Silicone Rubber/POSS Composites.