Figure 17 a shows an increasing trend of R Sm as a function of n , then a stabilisation from a dozen of layers.
← all excerpts
Effect of process parameters on surface integrity in laser powder bed fusion of Ti-6Al-4V alloy.
1
—
—
Figure 17 a shows an increasing trend of R Sm as a function of n , then a stabilisation from a dozen of layers.