Flexural Strength and Flexural Modulus In the three-point flexural test performed to evaluate the mechanical properties, all groups containing QAMS showed a decreasing trend in flexural strength compared with the control group (66.34 ± 7.31 MPa); however, the differences were not statistically significant.
← all excerpts
Effect of Immersion in Quaternary Ammonium Methacryloxy Silane Mixed Monomer on the Mechanical Properties and Antibacterial Activity of a 3D-Printed Urethane Dimethacrylate Denture Base Resin.