highly significantp < 0.01
Specifically, a highly significant difference in elastic modulus was observed between specimens printed along the L and W paths ( p < 0.01), while specimens printed along the L path showed significant differences ( p < 0.01) compared to other printing paths in yield strength, and elongation at break.