Barely Significant
← all excerpts

Crack Development and Healing in Guar Gum Polymer-Modified Silty Clay Under Natural Wetting-Drying Cycles.

Polymers (Basel) · 2025 · PMC12787747 · PMID 41516798

1
hedged sentence
closest p
boldest claim

The sentences

a decreasing trendno p-value reported
As shown in Figure 12 , both the fractal dimension of crack area and the fractal dimension of crack length exhibit a decreasing trend with increasing wetting–drying cycles, with R 2 > 0.94, indicating excellent model fitting performance.

also in 47,180 other papers

Quoted from the open-access full text in Europe PMC under the licence the publisher applied. The sentence is reproduced exactly as published; the emphasis is ours.