Comparative analysis of triple helices containing unmodified, 4-hydroxylated, and 4-fluorinated Pro residues revealed a decreasing trend in melting temperature in the order: PFlG (91°C) > PO 4 G (61°C) > PPG (41°C) ( Figure 3 ) [ 27 ].
← all excerpts
Molecular foundations of collagen triple helical assembly: the central role of prolyl-4-hydroxylation.