In contrast, the Primitive structure shows an unexpected trend, where maximum strength (28.35 MPa) is achieved at a 45% fraction, while at a 55% fraction there is a slight decrease to 27.41 MPa.
← all excerpts
The Effect of Non-Uniform Material Distribution on the Bending Strength and Energy Absorption of TPMS Structures.