The compressive strengths of CFSAG mix 4-A, 4-B and 4-C showed a decreasing trend with increased aeolian sand dosage at different maintenance temperatures.
← all excerpts
Durability and damage evolution of cement-fly ash stabilized aeolian sand gravel under high-temperature curing and freeze-thaw cycles.