The calculated bandgap values, consistent with the experimental measurements, exhibit a decreasing trend as the number of N defects increases, with values of approximately 1.15 and 0.90 eV for 1N and 2N defects, respectively ( Figure S2 ).
← all excerpts
Synergistic Defect-Piezoelectric Modulation of C<sub>3</sub>N<sub>5</sub> for Scalable On-Site Hydrogen Production.