As shown, both the flexural and compressive strengths exhibit a decreasing trend when the CRA content reaches 20%, with the flexural strength dropping from 7.35 to 4.12 MPa and the compressive strength decreasing from 16.26 to 10.71 MPa.
← all excerpts
A Novel Approach to Optimize the Rheology and Buildability of 3D-Printed Magnesium Phosphate Cement Composites Using Carbonated Recycled Aggregate.
1
—
—