(1) Different Starting Materials Affect Compressive Strength With the increase of sodium silicate modulus, the compressive strength showed a decreasing trend, and the 7-day and 28-day compressive strengths were 5.1 MPa and 6.1 MPa, respectively, at the sodium silicate modulus of 1.2.