Barely Significant
← all excerpts

Effect of Hydrogen Charging Current Density on Hydrogen Trapping Behavior in Cu6.01Ni2.7Mn Steel.

Materials (Basel) · 2026 · PMC13117093 · PMID 42073688

1
hedged sentence
closest p
boldest claim

The sentences

a decreasing trendno p-value reported
It can be observed that the lag time ( t lag ) for hydrogen atoms to penetrate the specimen exhibits a decreasing trend, declining from 862.2 s to 603.6 s.

also in 47,180 other papers

Quoted from the open-access full text in Europe PMC under the licence the publisher applied. The sentence is reproduced exactly as published; the emphasis is ours.