The degradation percentage over time follows a decreasing trend, with 4.0 wt% MgO–CuO/GO showing the highest degradation rate.
← all excerpts
GO-enhanced photocatalytic breakdown of emamectin benzoate by an MgO-CuO nanocomposite under visible light illumination.