Both the toughness and the Young's modulus also demonstrated an increasing trend compared to 2.719 MJ/m 3 and 16.35 MPa as the [2]catenane content is raised (Figure 3f ).
← all excerpts
Facile Preparation of a Poly[2]Catenane Network Using Self-Assembled [2]Catenane Unit.