The sentences

a decreasing trendno p-value reported
As shown in Figure a–c, at RH = 50%, 60%, and 70%, the fracture strains­(ε u ) of CNT/C–S–H reached 0.338, 0.312, and 0.297, respectively, which were substantially higher than the corresponding fracture strain of the C–S–H system (i.e., 0.272, 0.252, and 0.251). Moreover, the fracture strain of the CNT/C–S–H system exhibited a decreasing trend with increasing RH.

also in 47,180 other papers

Quoted from the open-access full text in Europe PMC under the licence the publisher applied. The sentence is reproduced exactly as published; the emphasis is ours.