At a fixed flowability, the water-to-solid ratio exhibited an increasing trend with an increase in GGBS fraction, rising from 0.337 ± 0.017 at 0% GGBS to 0.375 at 18% GGBS.
← all excerpts
Composition Design and Solidification Mechanism Analysis of Controlled Low-Strength Materials Using Stabilized Stainless Steel Mud.
2
—
—
The sentences
With the increase in GGBS fraction, the compressive strengths of CLSM at all ages exhibited a decreasing trend, which was generally consistent with the fact that the early reaction rate is relatively low and strength development is limited under the low-cement condition with GGBS.