Overall, a decreasing trend of α-helical content was observed for BSA from the native state (52%–68%)>adsorbed state (34%–42%)>released state (35%–39%)>powdered state (32%).
← all excerpts
Structural and functional characterization of proteins adsorbed on hydrophilized polylactide-co-glycolide microfibers.