a trend towards significanceP = 0.078
Furthermore only the β -TCP/PMMA scaffold had a significantly higher mineral volume present in the defect region compared to the autograft treatment ( Figure 4(e) ) ( P = 0.037); the mineral volume of the β -TCP scaffold showed a trend towards significance ( Figure 4(e) ) ( P = 0.078).