43 − 45 The remaining BCC superlattice exhibits a fairly significant lattice expansion at that point ( a BCC (190 °C after 340 s) = 4.16 nm), most likely due to the incorporation of ligands that have desorbed from the sintered regions of the superlattice.
← all excerpts
Role of Halides in the Ordered Structure Transitions of Heated Gold Nanocrystal Superlattices.