All samples showed improvement in toughness when sintered ≥1300°C, except for the 0.3 wt% doped samples, which in contrast displayed a decreasing trend up till 1450°C.
← all excerpts
The Effect of Cerium Oxide Addition on the Properties and Behavior of Y-TZP.