The reduction in strength was highly significant for D1 specimen, with the decrease of 11% to 64%, than for D2 specimen with the decrease of 0% to 33%.
← all excerpts
Effects of Nitrogen and Tensile Direction on Stress Corrosion Cracking Susceptibility of Ni-Free FeCrMnC-Based Duplex Stainless Steels.