Figure 4f shows an increasing trend of failure displacement for the grease- or oil-modified layers, but the failure displacement for dry-contact decreased as the velocity increased.
← all excerpts
Modification of the contact surfaces for improving the puncture resistance of laminar structures.
2
—
—
The sentences
The variation tendencies of peak load and energy dissipation also started with a decreasing trend, followed by an increasing trend as the velocity increased, similarly to the results of single-layer configurations.