For CEM III grouts, the capacitance C 2 reached its first maximum at 50 days, and it fell from that age to 120 days, rising from then until 150 days approximately, when it showed a decreasing trend in general terms.
← all excerpts
Long-Term Behaviour of Fly Ash and Slag Cement Grouts for Micropiles Exposed to a Sulphate Aggressive Medium.