highly significantP < 0.0002
However, at higher HA wt% (50 and 75), there was a large, highly significant increase in compressive modulus (13.7 and 33.6 MPa, respectively, P < 0.0002 for both).
However, at higher HA wt% (50 and 75), there was a large, highly significant increase in compressive modulus (13.7 and 33.6 MPa, respectively, P < 0.0002 for both).