The difference between all the groups was highly significant and more amount of adhesive was left on acid etched followed by the 1.5 W/20s laser-etched group.
← all excerpts
Comparison of surface roughness of enamel and shear bond strength, between conventional acid etching and erbium, chromium-doped: Yttrium scandium-gallium-garnet laser etching - An <i>in vitro</i> study.