3(f) shows a decreasing trend as the distance from the defect increases with maximal depth going from ≈25 nm to ≈2 nm and interposed minimal depths ranging from ≈6 nm to ≈0 nm.
← all excerpts
Analysis of nascent silicon phase-change gratings induced by femtosecond laser irradiation in vacuum.
1
—
—