highly significantP < 0.05
The different surface treatment groups showed highly significant differences ( P < 0.05), whereas the resin cement subgroups showed no significant differences ( P > 0.05).
The different surface treatment groups showed highly significant differences ( P < 0.05), whereas the resin cement subgroups showed no significant differences ( P > 0.05).