The tensile strength tests show an increasing trend, viz., 22.27, 22.96, 24.86, and 26.42 MPa, respectively, for CHAP-1, CHAP-3, NaCHAP-3, and NaCHAP-4 films, while the % tensile stresses of the CHAP-3, NaCHAP-3, and NaCHAP-4 films were found to be 8.88, 23.59, and 48.43%, respectively, higher than CHAP-1.
← all excerpts
Na-Montmorillonite-Dispersed Sustainable Polymer Nanocomposite Hydrogel Films for Anticancer Drug Delivery.