Tukey's post hoc test for MDP-containing Panavia F 2.0 Groups A2, B2, and C2 and META-containing G-CEM Groups A3, B3, and C3 revealed highly significant differences whereas comparison between Groups A1, B1, and C1 resin-modified glass ionomer RelyX luting showed no significant differences regardless of the surface treatment method used [ Table 2 ].
← all excerpts
An <i>in vitro</i> comparison of the effect of various surface treatments on the tensile bond strength of three different luting cement to zirconia copings.