However, the fracture zone shows an increasing trend with the increase in clearance and, therefore, even at 250 °C, the fracture zone value is observed to increase from approximately 0.043 mm at 10% clearance to approximately 0.11 mm at 30% clearance.
← all excerpts
Characterization of Sheared Edges in Warm Blanking of Magnesium Alloy AZ31B.
1
—
—