Clearly, R Ω , the resistance of the solution and electrode, presented a slightly increasing trend from 10.8 to 17.5 Ω/cm 2 under the potential of 1.2 to 1.6 V; meanwhile, the R ct, the charge transfer resistance, gave a decreasing trend from 277.4 to 168.6 Ω/cm 2 .
← all excerpts
Single atom tungsten doped ultrathin α-Ni(OH)<sub>2</sub> for enhanced electrocatalytic water oxidation.