At a relatively low reaction temperature (below 190 °C), the yield of LA exhibited an increasing trend and then reached the maximum value of 58% at 190 °C.
← all excerpts
Conversion of Sucrose into Lactic Acid over Functionalized Sn-Beta Zeolite Catalyst by 3-Aminopropyltrimethoxysilane.
2
—
—
The sentences
The maximum HMF yield (26%) over the Sn-Beta catalyst was obtained at 2 h, and then the HMF yield showed a decreasing trend with an increasing reaction time.